Hi all
Our grain pit is below the water table. The aging metal of the pit has resulted in a hairline crack that the water leaks through at a constant trickle.
Today we attempted to weld a plate over it with no success. The heat of the welder is boiling the water behind the steel and making the problem worse.
Does anyone have any ideas? Or any experience in this kind of problem.
Our grain pit is below the water table. The aging metal of the pit has resulted in a hairline crack that the water leaks through at a constant trickle.
Today we attempted to weld a plate over it with no success. The heat of the welder is boiling the water behind the steel and making the problem worse.
Does anyone have any ideas? Or any experience in this kind of problem.